1931-01-01

Prevention of Valve-Seat Erosion 310008

MORE THAN SEVEN YEARS of investigation of the problem of preventing valve-seat erosion under severe operating conditions in motor-truck and motorcoach engines are reviewed briefly. Engineers are said now to be generally agreed that an insert of some non-ferrous material is the only means of obtaining a valve seat that will stand severe service.
A theory for the cause of a thin spotty deposit or pick-up on the valve seat that accelerates erosion is advanced, and this deposit is said to be absent on valve seats made of non-ferrous metals. Aluminum bronze gives satisfactory results but is difficult to secure to cast-iron cylinder-blocks because of its greater coefficient of expansion.
Several partially successful methods of securing aluminum-bronze rings to cast iron are shown. A method that is applicable to one alloy which has reduced erosion under the most severe operating condition to such an extent that it is almost negligible is described.

SAE MOBILUS

Subscribers can view annotate, and download all of SAE's content. Learn More »

Access SAE MOBILUS »

Members save up to 16% off list price.
Login to see discount.
Special Offer: Download multiple Technical Papers each year? TechSelect is a cost-effective subscription option to select and download 12-100 full-text Technical Papers per year. Find more information here.
We also recommend:
TECHNICAL PAPER

A New Nissan 3.0-liter V-6 Twin-cam Twin-turbo Engine with Dual Intake and Exhaust Systems

900649

View Details

TECHNICAL PAPER

Development of Aluminium Hollow Subframe Using High-Pressure Die Casting

2016-01-0406

View Details

TECHNICAL PAPER

Overview of Sheet Metals for Stamping

970715

View Details

X