Safety Performance of Laminated Glass Configurations 670912

Impact performance of a large variety of interlayer combinations laminated with annealed plate, heat strengthened, and fully tempered glasses has been analyzed for acceleration pulses, “severity index,” and penetration. These tests, conducted at 0, 70, and 120 F, indicate that small interlayer thickness changes are most effective in upgrading performance. Severity index numbers well below 1000 were calculated for laminated safety glass with interlayer thickness as high as 0.120 in. Highly localized bending of glass panels during impact with the 22 lb headform has been recorded through high-speed photography as reflected grid board distortion. Lacerative potential of laminated safety glass is being evaluated by using a simulated tissue developed through studies of human tissue.

SAE MOBILUS

Subscribers can view annotate, and download all of SAE's content. Learn More »

Access SAE MOBILUS »

Members save up to 16% off list price.
Login to see discount.
Special Offer: Download multiple Technical Papers each year? TechSelect is a cost-effective subscription option to select and download 12-100 full-text Technical Papers per year. Find more information here.
We also recommend:
STANDARD

Specification and Inspection of Glass for Integrally Lighted Aerospace Instruments

ARP924B

View Details

STANDARD

Deodorant, Aircraft Toilet

AMS1476C

View Details

STANDARD

Core, Honeycomb, Glass/Phenolic Bias Weave Fiber Construction

AMS3716C

View Details

X