High Purity Magnesium AM60 Alloy: The Critical Contaminant Limits and the Salt Water Corrosion Performance 860288

Standard salt spray corrosion tests have been used with controlled purity AM60 castings to define the critical iron, nickel, and copper contaminant levels below which excellent corrosion performance can be obtained. As previously observed with the AZ91 alloy, the iron solubility and the corrosion tolerance limit for iron are dependent upon the manganese content of the metal. The zinc free AM60 alloy has a somewhat lower tolerance for all three of the critical contaminants when compared to AZ91, but when the three contaminants are below their individual tolerance limits, the salt spray performance is again equal to or better than die cast 380 aluminum and cold rolled steel.

SAE MOBILUS

Subscribers can view annotate, and download all of SAE's content. Learn More »

Access SAE MOBILUS »

Members save up to 16% off list price.
Login to see discount.
Special Offer: Download multiple Technical Papers each year? TechSelect is a cost-effective subscription option to select and download 12-100 full-text Technical Papers per year. Find more information here.
We also recommend:
TECHNICAL PAPER

Controlling the Salt Water Corrosion Performance of Magnesium AZ91 Alloy

850417

View Details

TECHNICAL PAPER

Composition and Performance of an Improved Magnesium AS41 Alloy

890205

View Details

TECHNICAL PAPER

Aluminum Wheel Alloy Variants: Effects on Corrosion Performance

980461

View Details

X