Development of Hydrogen Embrittlement Test Methods Which Reflect Realistic Maintenance Scenarios 983116

This paper compares several different test methods used to test maintenance chemicals for potential to induce hydrogen embrittlement in high-strength steel. The program was structured to accomplish three main objectives with regard to hydrogen embrittlement testing: 1) compare various test methods used to qualify maintenance chemicals, 2) compare various coatings used to protect high-strength steel parts such as landing gear, and 3) compare various high-strength steel substrates specified for aircraft landing gear. The coatings selected included electrodeposited cadmium (baseline), ion vapor deposited (IVD) aluminum, SermeTel 984, and Zinc-Nickel plate. Substrates tested included AISI 4340 (260-280 ksi HT), 300M (280-300 ksi HT), and AerMet 100 (minimum 290 ksi HT).

SAE MOBILUS

Subscribers can view annotate, and download all of SAE's content. Learn More »

Access SAE MOBILUS »

Members save up to 16% off list price.
Login to see discount.
Special Offer: Download multiple Technical Papers each year? TechSelect is a cost-effective subscription option to select and download 12-100 full-text Technical Papers per year. Find more information here.
We also recommend:
TECHNICAL PAPER

Zn-Ni Plating as a Cadmium Alternative

2007-01-3837

View Details

STANDARD

Plating, Brush, Nickel Low-Stress, Low-Hardness Deposit

AMS2451/3D

View Details

TECHNICAL PAPER

Ferritic Stainless Steels for Magnetic Applications

900384

View Details

X